PMMA 德国赢创德固赛 8NDF21通用注塑级 物性认证数据表
-
性能项目 |
测试条件 |
测试方法 |
数值/描述 |
单位 |
机械性能 |
拉伸强度(引张强度) |
|
ASTM D638/ISO 527 |
71 |
kg/cm²(MPa)[Lb/in2] |
断裂伸长率 |
|
ASTM D638/ISO 527 |
4.5 |
% |
拉伸模量 |
|
ASTM D638/ISO 527 |
3300 |
kg/cm²(MPa)[Lb/in2] |
拉伸屈服伸长率(延伸率) |
|
ASTM D638/ISO 527 |
|
% |
拉伸断裂伸长率(延伸率) |
|
ASTM D638/ISO 527 |
|
% |
弯曲模量(弯曲弹性率) |
|
ASTM D790/ISO 178 |
|
kg/cm²(MPa)[Lb/in2] |
弯曲强度 |
|
ASTM D790/ISO 178 |
|
kg/cm²(MPa)[Lb/in2] |
洛氏硬度 |
|
ASTM D785 |
|
|
IZOD 缺口冲击强度 |
1/4" 23℃ |
ASTM D256/ISO 179 |
18 |
kg·cm/cm(J/M)ft·lb/in |
1/4" -30℃ |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
1/8" 23℃ |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
1/8" -30℃ |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
Charpy冲击强度 |
23℃ (缺口) |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
-30℃(缺口) |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
23℃(无缺口) |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
-30℃(无缺口) |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
物性性能 |
比重(密度) |
|
ASTM D792/ISO 1183 |
|
|
成型收缩率 |
|
ASTM D955 |
|
% |
熔融指数(流动系数) |
200℃/5kg |
ASTM D1238/ISO 1133 |
|
g/10min |
220℃/10kg |
ASTM D1238/ISO 1133 |
2.5 |
g/10min |
吸水率 23℃/24H |
|
ASTM D570/ISO 62 |
|
% |
热性能 |
热变形温度 |
退火 |
ASTM D648/ISO 75 |
103 |
℃(℉) |
未退火 |
ASTM D648/ISO 75 |
|
℃(℉) |
维卡软化点 |
|
ASTM D1525/ISO R306 |
109 |
℃(℉) |
熔点 |
|
- |
|
℃(℉) |
燃烧性(率) |
|
UL94 |
|
|
线性膨胀系数 |
|
ASTM D696/ISO 11359 |
6.3 |
mm/mm.℃ |
电气性能 |
介电常数 |
100HZ |
ASTM D150/IEC 60250 |
|
|
1MHZ |
ASTM D150/IEC 60250 |
|
|
体积电阻率 |
|
ASTM D257/IEC 60093 |
|
Ω.cm |
表面电阻率 |
|
ASTM D257/IEC 60093 |
|
Ω |
耐电弧性 |
|
ASTM D495/IEC 60112 |
|
|
光学性能 |
折射率 |
|
ASTM D542/ISO 489 |
|
|
透光率 |
|
ASTM D1003/ISO 13468 |
87 |
% |
模糊系数(Haze) |
|
ISO 14782 |
|
% |
加工条件 |
干燥条件 |
|
|
|
|
加工温度 |
射嘴 |
|
|
℃ |
料筒前段 |
|
|
℃ |
料筒中段 |
|
|
℃ |
料筒后段 |
|
|
℃ |
熔体温度 |
|
|
|
℃ |
模具温度 |
|
|
|
℃ |
压力 |
注塑压力 |
|
|
Mpa |
保压压力 |
|
|
Mpa |
背压 |
|
|
Mpa |
螺杆转速 |
|
|
|
rpm |
其他 |
备注 |
|
颜色 |
|
特性 |
磨砂级 |
用途 |
|